Development of Austenitic Stainless Steel Cold-drawn Rods for Nuclear Power Plant Reactor Internals
Tan Qingfeng, Jia Hongshuai, Wang Yu, Yan Zhandong, Yun Yongjia, Wang Yuhui, Zheng Jihui
Special Steel . 2024, (3): 5 -9 .  DOI: 10.20057/j.1003-8620.2023-00207