Static CCT Curve Measurement and Microstructure Analysis of 18CrNiMo7-6 Steel
Lu Feng , Zhang Pei , Li Qi, Qiu Guoxing
Special Steel . 2024, (3): 91 -95 .  DOI: 10.20057/j.1003-8620.2023-00212