Effect of Nitrogen Content and Final Rolling Temperature on Low- temperature Impact Toughness of Titanium Microalloyed High- strength Steel CGLC700
Chen Yufeng, Zhang Junfen, Xue Qihe, Bai Jun, Yang Shufeng, Li Jingshe
Special Steel . 2024, (3): 40 -18 .  DOI: 10.20057/j.1003-8620.2023-00215