Application and Optimization of Mould Flow Field in 1000 mm-2200 mm Wide Slab Caster
Wang Yuping, Wu Jianbo
Special Steel . 2024, (5): 85 -89 .  DOI: 10.20057/j.1003-8620.2024-00072