ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Quenching Temperature on Mechanical Properties of M 6C Reinforced 2 200 MPa Ultra-high Strength Steel
Tang Yuanshou, Zhang Shiqing, Li Fang, He Qinsheng, Zhao Zhen, Wang Hong, Zou Xingzheng, Wang Jianqiao, Huang Yali
Special Steel . 2024, (5): 108 -112 .  DOI: 10.20057/j.1003-8620.2023-00204