Effect of Dual-aging Process on Microstructure and Properties of Co-precipitation Hardening Ultra-high Strength Steel
Zhao Jiawei, Tian Jialong, Yang Ping, Zhan Dongping, Jiang Zhouhua
Special Steel . 2024, (6): 88 -94 .  DOI: 10.20057/j.1003-8620.2024-00101