The Effect and Control of Rare Earth Ce on Carbonitrides Precipitation in 441 Ferritic Stainless Steel
Xie Kang, Mo Jinqiang, Zhang Wei, Wang Lijun
Special Steel . 2024, (6): 1 -7 .  DOI: 10.20057/j.1003-8620.2024-00073