Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel
Zheng Anmin, Fan Xuanyu, Huang Zengxin, Mao Wangwang, Yu Yanchong, Zhang Jinling, Wang Shebin
Special Steel . 2024, (6): 37 -47 .  DOI: 10.20057/j.1003-8620.2024-00138