Numerical Simulation of Flow and Solidification Behavior of Medium Mn steel in Thin Slab Mold
Tian Runyu, Song Bingjun, Peng Zhongyuan, Qiu Yarong, Kong Lingzhong, Yang Jie
Special Steel . 2025, (1): 48 -53 .  DOI: 10.20057/j.1003-8620.2024-00123