Effect of Aluminum Content on Microstructure and  Properties of Fe-1.4C-1.5Cr-Alx Steel
Shi Dafang, Yang Jun, Liu Dong, Wang Hui, Zhang Wanli, Yu Feng, Cao Wenquan
Special Steel . 2025, (1): 54 -58 .  DOI: 10.20057/j.1003-8620.2024-00115