Simulation of Central Porosity and Hot Crack Formation in 14 t Flat Ingot by Mold Removal Controlled Cooling
Wu Gang, Xu Changjun, Feng Xulong, Zhai Haodong, Xu Jichen, Hu Hanting
Special Steel . 2025, (1): 59 -65 .  DOI: 10.20057/j.1003-8620.2024-00155