ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Inclusion Evolution and Calcium Treatment Optimization of 9Ni Steel
Chen Dengguo, Lv Jiping, Wan Yong, Dong Fujun, Cao Ruihong, Sun Lefei
Special Steel . 2025, (1): 66 -74 .  DOI: 10.20057/j.1003-8620.2024-00188