The Influence of Direct Reduced Iron Size on EAF Smelting
Kang Xu, Cao Zhenwei, Wang Qiang, Liu Chong, Li Shuangjiang, Zhang Junfen
Special Steel . 2025, (1): 75 -78 .  DOI: 10.20057/j.1003-8620.2024-00184