ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Optimization of Electromagnetic Parameters for the 3rd-generation FC MOLD
Duan Fuchun, Wang Yuping, Zhu Zhiqiang
Special Steel . 2025, (1): 126 -133 .  DOI: 10.20057/j.1003-8620.2024-00161