Thermodynamic Coupling Analysis of Air Cooling for X70 Pipeline Steel Continuous Casting Slab Based on ABAQUS
Fu Chengzhe, Zhang Shuai, Wang Shuang, Gao Hong, Wang Fuyue, Zhang Zherui
Special Steel . 2024, (6): 62 -68 .  DOI: 10.20057/j.1003-8620.2024-00027