The Influence of Swirl Nozzle on the Flow Field in the Bloom Mould and the Interface Behavior of Steel Slag
Zhang Jianyu, Wang Xingjuan, Zhu Liguang, Song Yuanlong, Si Xulin, Zheng Xuelong
Special Steel . 2025, (2): 55 -61 .  DOI: 10.20057/j.1003-8620.2024-00216