ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Research on the Metallurgical Properties of Fluorine-Containing Refining Slag and Its Fluoride-Free Design
Li Haozhe, Jin Jinwen, Gao Fang, Gu Chao, Bao Yanpin, Wei Ze
Special Steel . 2025, (2): 72 -77 .  DOI: 10.20057/j.1003-8620.2024-00229