Study on the Effects of Partial Pressure on X52M Pipeline Hydrogen Embrittlement Properties in High-Pressure Hydrogen Environments
Zhao Qian, Liu Haixiao, Li Ming, Wang Bing, Li Ba, Jia Shujun, Liu Qingyou
Special Steel . 2025, (3): 117 -124 .  DOI: 10.20057/j.1003-8620.2024-00248