Effect of C and Mo Content on Microstructure and Short-term Properties of IN617 Heat-resistant Alloy
Liu Qicong, Jia Lei, Tang Zhengxin, Li Gen, Li Ling, He Guanze, He Xikou
Special Steel . 2025, (4): 71 -83 .  DOI: 10.20057/j.1003-8620.2025-00120