Effect of Two-stage Aging Time on Microstructure and Mechanical Properties of GH4706 Superalloy
Li Zhentuan, Huang Shuo, Wang Chong, Duan Ran, Qin Heyong, Zhao Guangpu
Special Steel . 2025, (4): 157 -162 .  DOI: 10.20057/j.1003-8620.2025-00069