ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Development and Practice of Nb-Ti Microalloying 750L Beam Steel by 120 t BOF-LF-CC Slab-8 mm Plate Flowsheet
Xu Zhengbiao, Wang Yanping, Liu Qisen, Xu Jian, Lin Chengjiang , Qin Zhe
Special Steel . 2021, (6): 43 -46 .