Research on Cracks Evolution of High Silicon Electrical Steel Fe-10 % Si and Low Carbon Steel Q235 Composite Plate in Rolling Process
Ji Shuai , Liu Zhongjun , Liang Kai , Gao Boyang , Zhao Minghui
Special Steel . 2021, (4): 1 -6 .