Diffusion Behavior of Nb and Si in GH2907 Alloy VIM + VAR 3 t Ingot During Homogenization Process at 1190 ℃
Wang Zhigang, Wen Jiali, Yang Guixin , Zheng Zhenyu , Liao Kai, Han Guangwei
Special Steel . 2021, (4): 17 -19 .