Improvement on Quality of Rolled Billet of EAF-LF-VD-CC Steelmaking High-Speed Railway Axle Steel DZ2 by Argon Shielding ESR
Zhang Jinwen, Wang Wenxian, Wu Zhonghua, Zhao Zhigang, Wang Songwei, Wang Zhixiang, Wang Yuling
Special Steel . 2021, (4): 25 -29 .