Influence of 120 t LF Stirring Intensity on Amount of Large Size Inclusions in Low Carbon Q195 Steel during Refining
Jiang Liping, Xu Jianfei, Yu Fei, Qu Zhidong
Special Steel . 2021, (4): 47 -50 .