Effect of Quenching and Tempering Heat Treatment on Microstructure and Mechanical Properties of 55NiCrMoV7 Die Steel
Zhao Jiquan , Qu Zhoude , Yu Xingsheng , Wu Chuan, Shi Ruxing
Special Steel . 2021, (4): 60 -65 .