Effect of Quenching and Tempering Treatment on Structure and  Mechanical Properties of 22MnCrNiMo Steel Flash Weld Zone
Li Zhongyu, Wang Xiaoguo, Dai Yibo, Zhang Yan , Guo Yuhang
Special Steel . 2021, (3): 71 -75 .