Effect of Deformation and Cooling Rate on Deformation-Induced  Ferrite Transformation in SCM435 Cold Heading Steel
Chen Jilin, Feng Guanghong, Yang Dong, Xue Zhengguo , Ma Honglei , Zhang Hongliang, Wang Baoshan, Ma Jian
Special Steel . 2021, (3): 12 -15 .