工作温度达 6 0 0℃。介绍了离子渗氮、N C共渗、N C V共渗、O S N共渗、S N C共渗、多元共渗等提高H13钢抗热疲劳、耐热磨损和耐蚀性能的表面低温化学热处理工艺
以及激光表面处理、高能束表面合金化、离子注入表面改性处理等高能束流表面处理及其最新进展。
Abstract
The steel H13(4Cr5MoSiV1)-0.32~0.45C
0.80~1.2Si
0.20~0.50Mn
4.75~5.50Cr
1.10~1.75Mo
0.80~1.20V is a hot-work die steel wide used for hot extrusion die and pressure casting die with service temperature up to 600 ℃.The surface low temperature thermo-chemical treatment including ion nitriding
nitrocarburizing
V- nitrocarburizing
sulpho-nitrocarburizing
oxy-sulpho-nitriding and multicomponent cementation to increase anti-thermal fatigue
thermo-wear abrasion and corrosion resistance is presented and the high energy density surface treatment including la- ser surface heat treatment
surface alloying with high energy density and surface modification with ion implantation and its development are reviewed in this paper.