Metallurgical Equipment and Process Route for Stainless Steel Steelmaking
更新时间:2026-01-21
    • Metallurgical Equipment and Process Route for Stainless Steel Steelmaking

    • Special Steel   Vol. 26, Issue 2, Pages: 28-31(2005)
    • Received:20 September 2004,

      Online First:29 May 2023,

      Published:29 May 2005

    移动端阅览

  • 郝祥寿. Metallurgical Equipment and Process Route for Stainless Steel Steelmaking[J]. Special Steel, 2005, 26(2): 28-31. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Key Metallurgical Technologies for Smelting 1Cr13 Stainless Steel via ANS-OB Process
Selection and Application of Cold Rolling Mill for Stainless Steel
Effect of Heat Treatment on Structure and Properties of A New Precipitation Hardening Stainless Steel 1Cr16Ni3Cu1MoW
Math Model for Optimum Charge Partition on Stainless Steel Smelting by K-OBM-S Process
A Study on Model of VOD Steelmaking Process for Stainless Steel

Related Author

Lu Zhihao
Teng Xingze
Xu Mengchun
Jin Zhe
Fu Xianbin
Li Boyang
王一德
高永亮

Related Institution

State Key Laboratory of Metallic Materials for Marine Equipment and Applications
Iron & Steel Research Institute of Ansteel Group
太原钢铁(集团)有限公司
昆明理工大学材料冶金工程学院
钢铁研究总院
0