Quality Control of Steel Blank for Tube of High Pressure Boiler by Concasting and Tandem Rolling at Xingcheng Special Steel
更新时间:2026-01-21
    • Quality Control of Steel Blank for Tube of High Pressure Boiler by Concasting and Tandem Rolling at Xingcheng Special Steel

    • Special Steel   Vol. 26, Issue 3, Pages: 61-62(2005)
    • Received:20 January 2005,

      Online First:30 May 2023,

      Published:30 May 2005

    移动端阅览

  • 葛龙桂, 李国忠. Quality Control of Steel Blank for Tube of High Pressure Boiler by Concasting and Tandem Rolling at Xingcheng Special Steel[J]. Special Steel, 2005, 26(3): 61-62. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Rare Earth Alloying Treatment of Hot Working Die Steel 3Cr2W8V
Practice of Steelmaking Process for of N80 Grade Steel 36Mn2V for Oil Well Tube Blank
A Study on Recrystallization of Non-Quenched-Tempered Steel 40Mn2V during Thermal Deformation

Related Author

陈列
佐辉
苗红生
尹良求
雷秀华
邓通武
方剑
邹喜洋

Related Institution

西宁特殊钢股份有限公司
攀枝花钢铁有限责任公司钢铁研究院
武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
湖南衡阳华菱钢管(集团)有限公司技术中心
0