Numerical Simulation of Temperature Field of Mould Copper Plate for Slab Continuous Casting
|更新时间:2026-01-21
|
Numerical Simulation of Temperature Field of Mould Copper Plate for Slab Continuous Casting
Special SteelVol. 26, Issue 1, Pages: 12-15(2005)
作者机构:
作者简介:
基金信息:
DOI:
CLC:
Received:25 July 2004,
Online First:24 May 2023,
Published:24 May 2005
稿件说明:
移动端阅览
冯科, 徐楚韶, 陈登福, et al. Numerical Simulation of Temperature Field of Mould Copper Plate for Slab Continuous Casting[J]. Special Steel, 2005, 26(1): 12-15.
DOI:
冯科, 徐楚韶, 陈登福, et al. Numerical Simulation of Temperature Field of Mould Copper Plate for Slab Continuous Casting[J]. Special Steel, 2005, 26(1): 12-15.DOI:
Numerical Simulation of Temperature Field of Mould Copper Plate for Slab Continuous Casting
In accordance with optimum revamping of structure of mould copper plats for a 1400mm X 170mm slab con- caster
a numerical simulation for 3- dimensional temperature fields of mould copper plats with two kinds of copper plate and immersed nozzle structure parameters before and after revamping has been studied by finite difference control volume method
The results obtained by simulation showed that the heat transfer effects of copper plate for wide face of mould obviously increased by optimum revamping with bolts gap modified from 160mm to 135mm and cooling water channel number modified from 65 to 55
with costing speed 1.4 m/min
at region nearby meniscus
the waximum temperature of inner and out curved wide face copper plate of mould after revamping respectively decreased by 15
^2 and 16
^0 as compared with that of mould before revamping.