您当前的位置:
首页 >
文章列表页 >
Current Status and Future Prospectus of Production and Development of Electrical Sheet Steel
更新时间:2026-01-21
    • Current Status and Future Prospectus of Production and Development of Electrical Sheet Steel

    • Special Steel   Vol. 26, Issue 1, Pages: 38-41(2005)
    • Received:20 July 2004,

      Online First:24 May 2023,

      Published:24 May 2005

    移动端阅览

  • 刘光穆, 刘继申, 谌晓文, et al. Current Status and Future Prospectus of Production and Development of Electrical Sheet Steel[J]. Special Steel, 2005, 26(1): 38-41. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Present Status and Development of Continuous Casting Technology for Special Steel in China
Production and Development of Wire for Steel Cord of Tyre
Application and Development of AOD Process for Stainless Steel Refining
Recent Progress on Electroslag Remelting Technology

Related Author

干勇
王忠英
余蓉
吴玮
郭永铭
张新宝
刘闯
姜周华

Related Institution

宝山钢铁股份公司特殊钢分公司
宝钢工程技术有限公司冶炼部
东北大学材料与冶金学院
北京钢铁研究总院.
0