Mathematical Modeling of K-OBM-S Converter Melting Process for Steelmaking of Stainless Steel
|更新时间:2026-01-21
|
Mathematical Modeling of K-OBM-S Converter Melting Process for Steelmaking of Stainless Steel
Special SteelVol. 27, Issue 2, Pages: 13-16(2006)
作者机构:
1. 东北大学材料与冶金学院,沈阳,110004
2. 太原钢铁集团有限责任公司,太原,030003
作者简介:
基金信息:
DOI:
CLC:
Received:12 October 2005,
Online First:24 February 2023,
Published:24 February 2006
稿件说明:
移动端阅览
董艳伍, 姜周华, 龚伟, et al. Mathematical Modeling of K-OBM-S Converter Melting Process for Steelmaking of Stainless Steel[J]. Special Steel, 2006, 27(2): 13-16.
DOI:
董艳伍, 姜周华, 龚伟, et al. Mathematical Modeling of K-OBM-S Converter Melting Process for Steelmaking of Stainless Steel[J]. Special Steel, 2006, 27(2): 13-16.DOI:
Mathematical Modeling of K-OBM-S Converter Melting Process for Steelmaking of Stainless Steel
建立了适用于80 t K-OBM-S转炉冶炼不锈钢的数学模型。对二步法冶炼2Cr13型不锈钢和三步法冶炼0Cr18Ni9型不锈钢的过程验证结果表明
大部分终点碳含量的误差≤±0.03%
终点铬含量误差≤±0.3%
110炉0Cr18Ni9钢目标碳(0.10%~0.25%)命中率为95.6%
终点目标铬(17.1%17.6%)的命中率为85.2%。
Abstract
K-OBM-S converter is a refining unit for steelmaking of stainless steel by charging hot metal and EAF premelting molten steel* Based on model of top-blown oxygen in converter for plain carbon steel melting and model of AOD process for stainless steel melting
a mathematical modeling of a 80 t K-OBM-S converter for steelmaking of stainless steel has been established. The verified results of steelmaking 2Crl3 stainless steel by duplex route and steelmaking 0Crl8Ni9 stainless steel by triplex route showed that the error of endrpoint carbon was mostly w ±0.03% and the error cf end-point chromium was ≤±0.3%
the percentage of hits for end-point aim caihon (0.10% - 0.25%) for 110 heats 0Crl8Ni9 steel was 95.6% and for end-point chromium (17.1% ~ 17.6%) was 85.2%