Advance on Process Technology of Extra-deep Drawing-Interstitial Atom Free (IF) Sheet Steel
更新时间:2026-01-21
    • Advance on Process Technology of Extra-deep Drawing-Interstitial Atom Free (IF) Sheet Steel

    • Special Steel   Vol. 26, Issue 2, Pages: 1-61(2005)
    • Online First:01 April 2005,

      Published:01 April 2005

    移动端阅览

  • 张鹏, 汪凌云, 任正德. Advance on Process Technology of Extra-deep Drawing-Interstitial Atom Free (IF) Sheet Steel[J]. Special Steel, 2005, 26(2): 1-61. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Development of Process for Φ55~70 mm Bar of GCr15 Bearing Steel Produced by 220 mm×220 mm Continuous Billet
Analysis on Sticking Defect of CSP Cold Rolled Steel Sheet Annealing in Bell Type Annealing Furnace
Development and Application of Lubrication Technology for Rolling Process
Analysis and Control of White Spots Defect on Strip of 316L Stainless Steel for Tank Container
Annealing Process and Product Characteristics of Baosteel's Semi-process Non-oriented Electrical Steel with Coating

Related Author

池武
计云萍
金自力
王权
张晓燕
任慧平
马艳丽
孙建林

Related Institution

上海交通大学材料科学与工程学院
内蒙古科技大学材料与冶金学院
包钢薄板厂
北京科技大学材料科学与工程学院
宝武集团山西太钢不锈钢股份有限公司冷轧厂
0