Determination of Capacity and Technical Parameters of Transformer for Ultra-High Power Electric Arc Furnace
|更新时间:2026-01-21
|
Determination of Capacity and Technical Parameters of Transformer for Ultra-High Power Electric Arc Furnace
Special SteelVol. 26, Issue 2, Pages: 35-37(2005)
作者机构:
1. 东北大学材料与冶金学院,沈阳,110004
2. 长春电炉有限责任公司,长春,130031
作者简介:
基金信息:
DOI:
CLC:
Received:14 September 2004,
Online First:29 May 2023,
Published:29 May 2005
稿件说明:
移动端阅览
阎立懿, 肖玉光, 王立志, et al. Determination of Capacity and Technical Parameters of Transformer for Ultra-High Power Electric Arc Furnace[J]. Special Steel, 2005, 26(2): 35-37.
DOI:
阎立懿, 肖玉光, 王立志, et al. Determination of Capacity and Technical Parameters of Transformer for Ultra-High Power Electric Arc Furnace[J]. Special Steel, 2005, 26(2): 35-37.DOI:
Determination of Capacity and Technical Parameters of Transformer for Ultra-High Power Electric Arc Furnace
steelmaking process and production flow sheet influence the determination of rating capacity of transformer for electric arc furnace
It has been obtained by analysis that for ultra-high power (UHP) electric arc furnace using scrap charging the relation fbnnula between rating capacity of transformer P
n
and parameters- electric power consumption W
transformer power utilization ratio G
total power.on time and steel tapping tonnage W is P
n
= (W*G
60)/(t
on
·cosφ·C
2
),and the setting method of transformer's secondary voltage is given. Combined with high-impedance techniques
the methods to determine the reactance capacity and transformer technical parameters of UHP electric arc furnace and the idea to determine the section
of graphite electrode are presented in this paper.