您当前的位置:
首页 >
文章列表页 >
Process Practice of AOD Refining for High Nitrogen Austenite Stainless Steel 1Cr22Mn15N
更新时间:2026-01-21
    • Process Practice of AOD Refining for High Nitrogen Austenite Stainless Steel 1Cr22Mn15N

    • Special Steel   Vol. 26, Issue 2, Pages: 51-53(2005)
    • Received:28 September 2004,

      Online First:31 May 2023,

      Published:31 May 2005

    移动端阅览

  • 高亦斌, 陈根保, 金卫强. Process Practice of AOD Refining for High Nitrogen Austenite Stainless Steel 1Cr22Mn15N[J]. Special Steel, 2005, 26(2): 51-53. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Process Practice for Increasing Lining Life of 45 t AOD Units
AOD Smelting of Austenitic Stainless 1Mn18Cr18N Protective Ring Steel
Practice for Refining Process of 92 t Ladle Furnace for Tube Bloom Steel J55
Process Practice of a 90 t Ladle Wire Feeding
Practice of Process for Decreasing Large Size Globular Oxides Inclusion (Ds) in Bearing Steel and Gear Steel

Related Author

王贵平
范红军
Xu Rongchuan
Guo Chang
Xu Yong
Zhang Xiaolei
Pan Mingxu
Zhang Donghai

Related Institution

太原钢铁(集团)有限公司
Forging Department, Daye Special Steel Co., Ltd.
攀钢集团成都钢铁有限责任公司
包头钢铁(集团)公司炼钢厂
江阴兴澄特种钢铁有限公司花山分厂三炼钢(1),质量检验中心(2),江阴
0