A Study on Behavior of Hot Deformation of Ultra- Low Carbon Nb-V-Ti Microalloyed Steel
更新时间:2026-01-21
    • A Study on Behavior of Hot Deformation of Ultra- Low Carbon Nb-V-Ti Microalloyed Steel

    • Special Steel   Vol. 26, Issue 3, Pages: 15-18(2005)
    • Received:12 December 2004,

      Online First:11 May 2023,

      Published:11 May 2005

    移动端阅览

  • 周家林, 唐力, 任勇, et al. A Study on Behavior of Hot Deformation of Ultra- Low Carbon Nb-V-Ti Microalloyed Steel[J]. Special Steel, 2005, 26(3): 15-18. DOI:

  •  
  •  