Numerical Simulation on Fluid Field in Mould for Slab Concasting
更新时间:2026-01-21
    • Numerical Simulation on Fluid Field in Mould for Slab Concasting

    • Special Steel   Vol. 26, Issue 2, Pages: 12-15(2005)
    • Received:18 October 2004,

      Online First:24 April 2023,

      Published:24 April 2005

    移动端阅览

  • 孙于萍, 李杰, 乐可襄, et al. Numerical Simulation on Fluid Field in Mould for Slab Concasting[J]. Special Steel, 2005, 26(2): 12-15. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Application and Optimization of Mould Flow Field in 1 000 mm-2 200 mm Wide Slab Caster
Effect of Inner Cooling Apparatus -U Shape Pipe on Flow of Molten Steel in Slab Continuous Casting Mold
Numerical Simulation of Flow Field of Molten Steel in Tundish for Slab Concasting and Operation Optimization
Numerical Simulation of Fluid Flowing in Concasting Mould for Wide Slab
A Study on Heat Flux and Temperature of ASP Concasting Mould Copper Plate

Related Author

Wu Jianbo
Wang Yuping
晋艳娟
崔小朝
贾凌锋
孙于萍
乐可襄
沈巧珍

Related Institution

Steel-making Plant,Bengang Steel Plates Co., Ltd.
太原科技大学应用科学学院
安徽工业大学冶金与资源学院
武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
武汉钢铁(集团)公司第三炼钢厂
0