Present Status and Development of Continuous Casting Technology for Special Steel in China
更新时间:2026-01-21
    • Present Status and Development of Continuous Casting Technology for Special Steel in China

    • Special Steel   Vol. 26, Issue 3, Pages: 1-5(2005)
    • Received:23 November 2004,

      Online First:10 May 2023,

      Published:10 May 2005

    移动端阅览

  • 干勇, 王忠英. Present Status and Development of Continuous Casting Technology for Special Steel in China[J]. Special Steel, 2005, 26(3): 1-5. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Current Status and Future Prospectus of Production and Development of Electrical Sheet Steel
Production and Development of Wire for Steel Cord of Tyre
Application and Development of AOD Process for Stainless Steel Refining
Recent Progress on Electroslag Remelting Technology
Equipment Characteristics and Practice of Continuous Casting Process for Large Round Bloom of Special Steels at Huaigang

Related Author

刘光穆
刘继申
谌晓文
刘新和
余蓉
吴玮
郭永铭
张新宝

Related Institution

宝山钢铁股份公司特殊钢分公司
宝钢工程技术有限公司冶炼部
东北大学材料与冶金学院
北京钢铁研究总院.
江苏沙钢集团淮钢特钢股份有限公司
0