Practice for Energy Saving of a 65 t Consteel Electric Arc Furnace by Hot Metal Charging at Shiheng Special Steel
|更新时间:2026-01-21
|
Practice for Energy Saving of a 65 t Consteel Electric Arc Furnace by Hot Metal Charging at Shiheng Special Steel
Special SteelVol. 26, Issue 2, Pages: 58-59(2005)
作者机构:
济南钢铁集团石横特殊钢厂,肥城,271612
作者简介:
基金信息:
DOI:
CLC:
Received:17 December 2004,
Online First:01 June 2023,
Published:01 June 2005
稿件说明:
移动端阅览
李洪勇, 柴建铭, 姚娜. Practice for Energy Saving of a 65 t Consteel Electric Arc Furnace by Hot Metal Charging at Shiheng Special Steel[J]. Special Steel, 2005, 26(2): 58-59.
DOI:
李洪勇, 柴建铭, 姚娜. Practice for Energy Saving of a 65 t Consteel Electric Arc Furnace by Hot Metal Charging at Shiheng Special Steel[J]. Special Steel, 2005, 26(2): 58-59.DOI:
Practice for Energy Saving of a 65 t Consteel Electric Arc Furnace by Hot Metal Charging at Shiheng Special Steel