您当前的位置:
首页 >
文章列表页 >
Water Modelling Test on Bath Mixing Behavior for CAS Powder Injection Refining
更新时间:2026-01-21
    • Water Modelling Test on Bath Mixing Behavior for CAS Powder Injection Refining

    • Special Steel   Vol. 28, Issue 3, Pages: 13-15(2007)
    • Received:08 November 2006,

      Online First:31 January 2023,

      Published:31 January 2007

    移动端阅览

  • 赵成林, 李建伟, 邹宗树. Water Modelling Test on Bath Mixing Behavior for CAS Powder Injection Refining[J]. Special Steel, 2007, 28(3): 13-15. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study of Water Modelling on Mixing Time for a 300 t Hot Metal Desulphurization-Pretreated by Double-Lance Injection Process
The Influence of Swirl Nozzle on the Flow Field in the Bloom Mould and the Interface Behavior of Steel Slag
Numerical Simulation of Bottom Argon Blowing Process for 130 Ton Ladle
Research and Application Progress of Plasma Heating Technology for Continuous Casting Tundish
A Study of Water Model on Mixing Characteristics of Powder Injected through Top Lance in RH-PTB Vacuum Refining Unit

Related Author

庞在刚
张炯明
叶凡新
任嵬
Song Yuanlong
Zheng Xuelong
Si Xulin
Zhu Liguang

Related Institution

北京科技大学冶金与生态工程学院
School of Metallurgy and Energy, North China University of Science and Technology
College of Materials and Engineering, Hebei University of Science and Technology
School of Metallurgical Engineering, Xi'an University of Architecture and Technology
Hebei Iron and Steel Group Shigang Company
0