Math Simulation for Process Energy Consumption of Scrap-EAF Flow Sheet and Hot Metal+ Scrap-EAF Flow Sheet
|更新时间:2026-01-21
|
Math Simulation for Process Energy Consumption of Scrap-EAF Flow Sheet and Hot Metal+ Scrap-EAF Flow Sheet
Special SteelVol. 28, Issue 3, Pages: 4-6(2007)
作者机构:
上海大学、上海市钢铁冶金重点实验室,上海,200072
作者简介:
基金信息:
DOI:
CLC:
Received:27 November 2006,
Online First:30 January 2023,
Published:30 January 2007
稿件说明:
移动端阅览
仇晓磊, 孟庆玉, 洪新. Math Simulation for Process Energy Consumption of Scrap-EAF Flow Sheet and Hot Metal+ Scrap-EAF Flow Sheet[J]. Special Steel, 2007, 28(3): 4-6.
DOI:
仇晓磊, 孟庆玉, 洪新. Math Simulation for Process Energy Consumption of Scrap-EAF Flow Sheet and Hot Metal+ Scrap-EAF Flow Sheet[J]. Special Steel, 2007, 28(3): 4-6.DOI:
Math Simulation for Process Energy Consumption of Scrap-EAF Flow Sheet and Hot Metal+ Scrap-EAF Flow Sheet
Based on materials balance model and heat balance model and combined with relative process parameters
the calculated models for process energy consumption of scrap-arc fumace steelmaking-concasting-continuous rolling(scrap- EAF)flow sheet and hot metal +scrap-arc fumace-concasting-continuous rolling(metal+ scrap-EAF)flow sheet have been established and the effect of several key parameters on process energy consumption is analyzed. Results showed that compared with scrap-EAF flow sheet the process energy consumption of 33% metal+ scrap-EAF increased by 43.72 kg
ce
/t
stsel
but its total energy consumption of flow sheet increased by 1/3.