Wear Resistance and Wearing Mechanism of Three Kinds of Corrosion Resistant Plastic Die Steel
更新时间:2026-01-21
    • Wear Resistance and Wearing Mechanism of Three Kinds of Corrosion Resistant Plastic Die Steel

    • Special Steel   Vol. 28, Issue 5, Pages: 37-39(2007)
    • Received:08 May 2007,

      Online First:14 February 2023,

      Published:14 February 2007

    移动端阅览

  • 颜飞, 徐洲, 金冰忠. Wear Resistance and Wearing Mechanism of Three Kinds of Corrosion Resistant Plastic Die Steel[J]. Special Steel, 2007, 28(5): 37-39. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Grain Growth Behavior of Nickel-based Superalloy GH3230
The As-Cast Microstructure and Solidification Segregation Behavior of GH5188 Alloy Produced by VIM+ESR Dual Melting Process
Control of Carbides and Process Optimization in the Direct Rolling Process of Cr12MoV Flat Steel
Development Process of Cutter Ring for Shield Machine/Tunnel Boring Machine (TBM) Hob
Effect of Solution Temperature on Microstructural Evolution and Tensile Properties of Hot-rolled Haynes 230 Alloy Bar

Related Author

Zhang Xin
Zhang Bingbing
Shang Shuming
Zhen Xingmin
Kou Jinfeng
Bai Yaguan
Nie Yihong
Zhou Yun

Related Institution

Capital Aerospace Machinery Co., Ltd.
China First Heavy Industries
Heilongjiang Provincial Key Laboratory of Intelligent Manufacturing for Advanced Nuclear Power Equipment
Tianjin Heavy Industries Research & Development Co., Ltd.
Songshan Lake Materials Laboratory, Dong guan
0