Finite Element Analysis on Rolling Load Parameters of Hot Continuous Mandrel Rolling of T91 Steel Seamless Tube
更新时间:2026-01-21
    • Finite Element Analysis on Rolling Load Parameters of Hot Continuous Mandrel Rolling of T91 Steel Seamless Tube

    • Special Steel   Vol. 27, Issue 5, Pages: 3-5(2006)
    • Received:20 March 2006,

      Online First:01 October 2006,

      Published:01 October 2006

    移动端阅览

  • 洪慧平, 赵志毅, 康永林, et al. Finite Element Analysis on Rolling Load Parameters of Hot Continuous Mandrel Rolling of T91 Steel Seamless Tube[J]. Special Steel, 2006, 27(5): 3-5. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study on Decarburization Trend of New High Strength and Toughness Spring Steels 40T and 44T
A Study on Oxygen Contamination from Crucible Material on Molten Steel during Vacuum Induction Melting
Metallurgy Technology for Ultra-Low Carbon and UItra- Low Nitrogen Steel
Effect of Heat Treatment on Properties of High Strength Spring Steel 60SiCrV7
Practice of Free Cutting Steel 35MnVS Steelmaking by 30t EAF-40t  LF

Related Author

尹钟大
徐德祥
刘德富
薛正良
高俊波
齐江华
李正邦
张家雯

Related Institution

哈尔滨工业大学
武汉钢铁(集团)公司技术中心
东北特钢集团北满特殊钢有限责任公司
新疆八一钢铁股份公司板带指挥部
本溪钢铁集团公司
0