您当前的位置:
首页 >
文章列表页 >
Effect of Hot Deformation on Structure and Microhardness of 0.05C-0.13Nb Steel
更新时间:2026-01-21
    • Effect of Hot Deformation on Structure and Microhardness of 0.05C-0.13Nb Steel

    • Special Steel   Vol. 29, Issue 1, Pages: 25-27(2008)
    • Received:09 July 2007,

      Online First:13 December 2022,

      Published:13 December 2008

    移动端阅览

  • 阴树标, 张志波, 孙新军, et al. Effect of Hot Deformation on Structure and Microhardness of 0.05C-0.13Nb Steel[J]. Special Steel, 2008, 29(1): 25-27. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Precipitate Behavior of Second Phase and Structure of Annealed 1.5 mm Cold Rolling Sheet of Nb-Ti Microalloy High Strength Steel
Effect of Finished Rolling Cooling Rate on Structure of Microalloy Non Quenched-Tempered Steel 34Mn2VN
Effect of Solution Temperature on Structure and Properties of 022Cr22Ni5Mo3N Duplex Stainless Steel
Effect of Cooling Rate on Structure Evolution of Hot Deformed Ferrite-Bainite Micro Alloying Steel
Effect of Quenching and Partitioning(Q & P)Process on Structure and Mechanical Properties of Steel 25Si2Ni3

Related Author

刘浩
陈晓
李平和
郑红
吴青松
刘清友
张玉胜
刘雅政

Related Institution

武汉科技大学材料与冶金学院
武汉钢铁公司技术中心
钢铁研究总院
北京科技大学材料学院
包钢集团公司无缝钢管厂
0