Experiment on Optimum Location of Bottom Nozzle in a 130 t Argon Stirred Ladle by Water Model
更新时间:2026-01-21
    • Experiment on Optimum Location of Bottom Nozzle in a 130 t Argon Stirred Ladle by Water Model

    • Special Steel   Vol. 28, Issue 4, Pages: 13-15(2007)
    • Received:30 December 2006,

      Online First:05 January 2023,

      Published:05 January 2007

    移动端阅览

  • 幸伟, 倪红卫, 沈巧珍, et al. Experiment on Optimum Location of Bottom Nozzle in a 130 t Argon Stirred Ladle by Water Model[J]. Special Steel, 2007, 28(4): 13-15. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Study of Water Model on Mixing Characteristics of Flow Field in CAS Ladle with Deep Inserting Snorkel
Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel
A Study on Physical Simulation for Liquid Flow in a New-Type Ladle at Xingcheng Special Steel
Water Modeling Examination for Optimization of Bottom Argon Blowing Location in 250 t Ladle Refining
A Study on Water Model for Optimum Process of Bottom Blowing Argon of 120 t Ladle

Related Author

干磊
何平
曾亚南
李俊国
韩志杰
李守章
吴雨晨
李红星

Related Institution

钢铁研究总院冶金工艺研究所,北京1
唐山钢铁股份有限公司
河北理工大学冶金与能源学院,唐11J
北京科技大学
兴澄特种钢铁有限公司,江阴
0