Effect of Cooling Rate on Structure Evolution of Hot Deformed Ferrite-Bainite Micro Alloying Steel
更新时间:2026-01-21
    • Effect of Cooling Rate on Structure Evolution of Hot Deformed Ferrite-Bainite Micro Alloying Steel

    • Special Steel   Vol. 28, Issue 3, Pages: 35-37(2007)
    • Received:22 December 2006,

      Online First:03 February 2023,

      Published:03 February 2007

    移动端阅览

  • 管丽, 刘雅政, 周乐育, et al. Effect of Cooling Rate on Structure Evolution of Hot Deformed Ferrite-Bainite Micro Alloying Steel[J]. Special Steel, 2007, 28(3): 35-37. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Thermal Simulation Study on Controlled Rolling and Cooling Process for Quality Spring 60Si2CrVAT
Structure Evolution of a Nb-Microalloyed Extra-Low Carbon Steel during Simulated Thermomechanical Control Process
Advance in Research on Evolution of Structure in TRIP Steels during TMP and Heat Treatment
Effect of Hot Deformation on Structure and Microhardness of 0.05C-0.13Nb Steel
Effect of Deformation and Cooling Rate on Deformation-Induced Ferrite Transformation in SCM435 Cold Heading Steel

Related Author

黄学启
崔娟
贺信莱
陈颜堂
付俊岩
侯豁然
郭爱民
唐代明

Related Institution

攀枝花学院四川省钒钛材料工程技术研究中心
昆明理工大学材料与冶金工程学院
钢铁研究总院结构材料研究所
河北省线材工程技术研究中心
邢台钢铁有限责任公司
0