Numerical Simulation of Fluid Flowing in Concasting Mould for Wide Slab
更新时间:2026-01-21
    • Numerical Simulation of Fluid Flowing in Concasting Mould for Wide Slab

    • Special Steel   Vol. 28, Issue 3, Pages: 7-9(2007)
    • Received:16 November 2006,

      Online First:30 January 2023,

      Published:30 January 2007

    移动端阅览

  • 沈巧珍, 朱必炼, 王俊杰, et al. Numerical Simulation of Fluid Flowing in Concasting Mould for Wide Slab[J]. Special Steel, 2007, 28(3): 7-9. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Application and Optimization of Mould Flow Field in 1 000 mm-2 200 mm Wide Slab Caster
Quality Defects of H Section Steel Continuous Casting and Numerical Simulation for Structure Optimization of Submerged Nozzle
Numerical Simulation of Transferring Characteristics of Liquid Steel in Mould for Continuous Casting H-Beam Bloom
Effect of Nozzle Angle on Flow Field in Mould for 150 nun x 380 nun Rectangular Bloom Casting
Numerical Simulation on Optimization of Inclination of Submerged Nozzle for 220mm x 1600mm Slab Casting and Application

Related Author

Wang Yuping
Wu Jianbo
李小明
史雷刚
崔雅茹
李文峰
阮飞
冯孔方

Related Institution

Steel-making Plant,Bengang Steel Plates Co., Ltd.
西安建筑科技大学冶金学院
内蒙古科技大学材料与冶金学院
上海大学上海市现代冶金与材料制备重点实验室
华北理工大学迁安学院,迁安
0