Effect of process factors oxygen supply rate and lance level on bath stirring
spitting and penetrating depth for 300 t converter melting has been simulated and studied by 1 • 13 water model. The water model test results showed that as Fr was controlled within 113. 1 and lance level was maintained at 0. 167 m (corresponding 300 t converter lance level 2. 17 m)
mixing time of bath reduced
spitting decreased during blowing
and better bath stirring effect was got with shallow penetrating depth to be available to decrease impact strength on furnace bottom.
A Study on Water Modeling Test of Tundish for Slab Concasting
Effect of 80 t Converter-Ladle Argon Stirring - Concasting Steelmaking Process on Gas and Inclusion Content in Steel Q235A
Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel
Effect of Converter-LF Refining and Hot Metal Pretreatment Converter-Ladle Argon Stirring Process on Metallurgical Quality of Weathering- Resisting Steel